Blog
15
2025
09
The process flow of powder coating equipment
1. **Pre-treatment**: **Purpose**: To remove oil, dust, and rust from the workpiece surface, while simultaneously forming a corrosion-resistant "phosphate coating" that enhances the adhesion of the subsequent spray coating. **Key Process Steps**: Degreasing, derusting, phosphating, and passivation. After pre-treatment, the workpiece not only becomes free of oil, rust, and dust but also develops an even, slightly rough, grayish phosphate film on its originally shiny white surface. This film effectively prevents rusting while significantly improving the adhesion of the powder coating. 2. **Electrostatic Spraying**: **Purpose**: To evenly apply a layer of powder coating onto the workpiece surface. For special parts—especially those prone to electrostatic shielding—a high-performance electrostatic powder coating machine is used. **Process Steps**: - Utilizing the principle of electrostatic attraction, a uniform layer of powder coating is sprayed onto the workpiece surface. - Excess powder that falls off is collected by a recovery system, sifted, and then reused. 3. **High-Temperature Curing**: **Purpose**: To heat the powder coating applied to the workpiece surface to a specified temperature and maintain it for a set duration, allowing the coating to melt, flow, and cure completely, thereby achieving the desired finish quality. **Process Steps**: - The coated workpiece is moved into a curing oven, where it is heated to the predetermined temperature (typically 185°C) and held at that temperature for the prescribed time (usually 15 minutes). - Once the process is complete, the workpiece is removed from the oven and allowed to cool naturally, resulting in the finished product. Note that different types of workpieces may require varying heating temperatures and curing times. **Tip**: The heating and control system—including electric, fuel-based, gas-fired, or coal-fired heating methods—functions as part of the insulated chamber, which serves as the curing oven. 4. **Cooling After Curing**: Cooling after curing involves reducing the temperature of the coated workpiece back to normal levels, ensuring it returns to room temperature safely and efficiently. 5. **Decorative Finishing**: **Purpose**: To achieve specific aesthetic effects on the workpiece after electrostatic spraying, such as wood grain patterns, decorative textures, or enhanced gloss finishes. **Process Steps**: - Applying clear-coat finishes or employing transfer printing techniques to enhance the visual appeal of the product. **Spray Coating Product Inspection Standards** 1. **Purpose**: To standardize the inspection process for spray-coated products, ensuring consistent and effective quality control across all production batches. 2. **Scope**: These standards apply to both laboratory testing and on-site quality control inspections of spray-coated products. **Requirements for Hardware Tool Spray-Coated Products**: 1. **Testing Methods for Prototype Spray-Coated Products**: For new or redesigned spray-coated products, initial inspection is conducted jointly by the Technical Department and the Inspection Department. The inspection verifies that the product’s structure meets design specifications and confirms that external silk-screen printing aligns with design requirements, including print location, color, size, and clarity. **Structural Inspection of Spray-Coated Products**: 1.1 **Basic Structural Requirements**: The dimensions and assembly of the spray-coated product must precisely match the design drawings, adhering to relevant technical specifications and national standards. 1.2 **Inspection Method for Product Structure**: After the product is sent for inspection, a functional test is performed using a corresponding semi-finished prototype. This step ensures the structural accuracy of the product and confirms that assembly is convenient and secure. If the first prototype fails inspection, a second unit must be tested. If both prototypes exhibit the same defects, the entire batch is considered non-compliant. 1.3 **Aesthetic Inspection of Spray-Coated Products**: Visual inspection is conducted using standard or corrected vision. 1.3.1 **Color Uniformity**: The sprayed color must match the selected sample or color chart exactly. After spraying, the product’s surface should display a uniform hue without noticeable color variations when viewed visually. 1.3.2 **Coating Thickness**: The thickness of the spray coating must meet both design and application requirements, ensuring even coverage and strong adhesion. 1.3.3 **Product Cleanliness**: All visible interior and exterior surfaces must be thoroughly clean, free from stains, grease, or any other contaminants that could detract from the product’s appearance. Additionally, no white residue should remain after a finger swipe across the surface. 1.3.4 **Inspection of Silk-Screen Printing**: Verify that the content and color of the silk-screen printing align precisely with the design specifications. Ensure the print is sharp, clear, and free from defects such as misprints, omissions, color mismatches, illegibility, or significant breaks in the printed lines. 1.3.5 **Defect Inspection of Spray-Coated Products**: 1.3.5.1 **Water Leakage and Rust Prevention**: Spray-coated products must be leak-proof. A waterproofing test is mandatory before final inspection. Randomly select 2% of each batch for this test: Place a sheet of toilet paper inside the product box, assemble the product by tightening the screws, seal the cap holes with tape, and then subject the assembled product to a 20-minute water spray from all sides (top, front, and back). Afterward, carefully dry the product and inspect the toilet paper. If the paper remains completely dry, the product passes the test. Alternatively, after the waterproofing test, examine the bottom of the box under bright light; there should be no visible light leakage through the corners or cracks, weld defects, or gaps. The upper and lower lids must fit tightly together, allowing easy assembly and disassembly. Internal rivet sleeves must remain securely fastened without loosening or falling out. If the first product fails this test, proceed to inspect the second unit. If both units fail, the entire batch is deemed non-compliant. 1.3.5.2 **Damage and Deformation**: The surface of the spray-coated product must be free from dents, scratches, or warping. Any unevenness, raised edges, or bent corners are unacceptable. 1.3.5.3 **Scratches**: Friction-related scratches are strictly prohibited, ensuring the product maintains a pristine, flawless appearance.1.3.5.4 Particles: The surface of the powder-coated product must not have large patches of small plastic powder particles, screen-printed ink dots, raised bumps, protruding marks, or flow marks. Dispersed and minor particle presence is allowed. 1.3.5.5 Pits: The surface of the powder-coated product should not feature extensive pits; however, scattered and trace amounts of pits are acceptable. 1.3.5.6 Scratches: The surface of the powder-coated product must be free from scratches, especially deep ones that expose the underlying material. Additionally, large areas of visible scratches are not permitted—only scattered and minimal scratch marks are allowed. 1.3.5.7 Gaps: Powder-coated products must be waterproof, and there are specific requirements for any gaps present. 2. Inspection Result Handling: For structural inspections of powder-coated products, if two out of two trial assemblies fail, the entire batch will be deemed non-compliant. If the pass rate for visual inspections of powder-coated products reaches or exceeds 95%, non-conforming items will be returned for rework. However, if the pass rate falls below 95%, the entire batch will be classified as non-compliant. In cases where a batch of powder-coated products fails inspection, an Non-Conformance Report must be completed and submitted to the Quality Control Center. Company Website: www.gzqxjd.com Contact Numbers: Ms. Wu: 18718849558 Ms. Liu: 13728095578 Company Address: No. 29-3 Hongqi Road, Zhuliao, Zhongluotan Town, Baiyun District, Guangzhou
Powder Coating Equipment, Spraying